31. The high efficiency anti-collapse asphalt powder consists of asphalt 62-75 wt%, softening point regulator 0-6 wt%, fluid loss reducing agent 20-35 wt%, and asphalt binding agent 0-5 wt%. 32. Tmis paper deals with the ordering of Fe - 1.83 C ( Wt % ) martensite during aging at roomtemperature. 33. Objective [ WT 6 BZ ] To study the clinical value of sandbag in sack hemorrhage of pacemaker implantation. 34. Objective : [ WT 5 BZ ] To compare the effect and safeness of benazepril and captopril in treatment of renal hypertension. 35. The change in AR , SRD 5 A 2, WT 1 genes and the anomaly chromosome may result in hypospadias. 36. So, the blends containing 7 wt% core-shell structured silicon rubber and 3 wt% compatibilizer can achieve a UL94 V-0 rating in vertical burning test. 36.try its best to gather and build good sentences. 37. Studies the function of wavelet transform (WT) that can effectively distill the transient characteristics of digital signals to estimate the symbol rate of PSK signals. 38. Exemplary LCD image mask glasses include fused silica, high purity fused silica and silica-titania containing 5-10 wt. % titania. 39. The stability of up - quenched Cu - 25 . 0 Zn - 4.20 Al ( wt . % ) alloy has been studied by positron annihilation and X - ray diffraction. 40. Recently, more and more practical applications show that in excessively noisy electromagnetic environment, using wavelet transform (WT) only may bring waveform distortion. 41. The results show that coupling the PET/Polyolefine blends by g not only enhances strongly the mol. wt. of PET, but also promotes the growth rate of PET crystallization. 42. In this paper, we discuss the relation between matched filter and wavelet transform(WT), and point out that wavelet transform is just the matched filter with changeable detection template. 43. The results indicate the physics characteristic of magnesium hydroxide was optimal when ADDP reaches 1 wt %. 44. Type : Whole synthetic resin ( QS ), Composite ( HH ), and Antiskid without pellet ( WT ). 45. The dry vibrating material is prepared with magnesite or forsterite in 85-97 wt% and sodium metasilicate in 3-15 wt%, and through mixing, vibration forming, stoving at 100-400 deg. c and demolding.